PHYSICAL PROPERTY | TEST STANDARD | VALUES | |
Hardness | Shore A | ASTM D2240 | 36+/-3 |
Specific Gravity | g/cm3 | ASTM D397 | 0.96 +/-0.03 |
Modulus@500% | Mpa | ASTM D412 | 2.1 |
Tensile Strength | Mpa | ASTM D412 | 23 Min |
Elongation | % | ASTM D412 | 780 Min |
Resilience | % | ASTM D5963 | 81 |
Tear Strength | N/mm | ASTM D624 | 40 Min |
Wet Abrasion | 103% | ||
Working Temperature | °C | -40 – +70 |